Yttrium stabilized tetragonal zirconia (YTZP) has opened up new prospects for all-ceramic restorations. However, one of the most common problems in the manufacture of zirconia prostheses is the violation of the integrity of frames and chipped ceramic tiles. In the process of manufacturing zirconium frames of fixed prosthesis there are elements of abrasion and heat treatment. However, it is likely that these effects may affect the mechanical properties of frames. Therefore aim of this study was to determine the nature and impact of the blast and mechanical processing of samples from stabilized zirconia, using diamond tools, as well as high-temperature re-firing on the properties of their strength and the phase state and determine the feasibility of regenerating firing to restore the original properties and the phase state of the material.

Full Text

Исследование влияния поверхностной абразивной обработки и температурного воздействия на свойства стоматологической керамики на основе мета-стабильного тетрагонального диоксида циркония
×

About the authors

Nina Amurkhanovna Tsalikova

References

  1. Komine F., Blatz M.B., Matsumura H. Current status of zirconia-based fixed restorations. J. Oral Sci. 2010; 52 (4): 531-9.
  2. Sailer I., FeherA., Filser F et al. Five-year clinical results of zirconia frameworks for posterior fixed partial dentures. Int. J. Prosthodont. 2007; 20: 383-8.
  3. Guazzato M., Albakry M., Quach L., Swain M.V. Influence of surface and heat treatments on the flexural strength of a glass-infiltrated alumina/zirconia-reinforced dental ceramic. Dent. Mater. - 2005; 21: 454-63.
  4. Kosmac T., Oblak C., Jevnikar P., Funduk N., Marion L. Strength and reliability of surface treated Y-TZP dental ceramics. J. Biomed. Mater. Res. 2000; 53 (4): 304-13.
  5. Sundh A., Molin M., Sjogren G. Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after venee ring and mechanical fatigue testing. Dent. Mater. 2005; 21: 476-82.

Supplementary files

Supplementary Files
Action
1. JATS XML

Copyright (c) 2013 Eco-Vector



СМИ зарегистрировано Федеральной службой по надзору в сфере связи, информационных технологий и массовых коммуникаций (Роскомнадзор).
Регистрационный номер и дата принятия решения о регистрации СМИ: серия ПИ № ФС 77 - 86295 от 11.12.2023 г
СМИ зарегистрировано Федеральной службой по надзору в сфере связи, информационных технологий и массовых коммуникаций (Роскомнадзор).
Регистрационный номер и дата принятия решения о регистрации СМИ: серия ЭЛ № ФС 77 - 80635 от 15.03.2021 г
.



This website uses cookies

You consent to our cookies if you continue to use our website.

About Cookies